Influence of Dye Loading Time on Zirconia Photoanode for Solar Cell Application

Bikram Prasad1, 2

Chaitali Jagtap1,*,Email

Vishal Kadam1

Sandesh Jadkar1

Habib Pathan1

1 Advanced Physics Laboratory, Department of Physics, Savitribai Phule Pune University, Pune, 411007, India
2 Department of Physics, Shri Mahanth Shatanand Giri College, Sherghati, Gaya, 824211, India

 

Abstract

To reduce the dependence on the non-renewable sources of energy and finding the new pathway to utilize the affordable renewable source of energy, the present study focusses on harnessing the sun’s radiation by a solar device, popularly known as dye sensitized solar cell (DSSCs). The DSSCs have been fabricated by using N3 dye as a sensitizer to sensitize the zirconia (ZrO2)/CL films, polyiodide as an electrolyte and platinum-coated fluorine-doped tin oxide (FTO) as a counter electrode. The ZrO2 paste was prepared and were deposited onto the compact layer of ZnO by the doctor blade technique. The presence of zinc oxide compact layer helps in improving the performance of the device by suppressing the recombination losses and thereby increasing the short circuit current and fill factor. The prepared crystalline films were dipped in the N3 dye for 6, 12, 18, and 24 hours at 300 K, which resulted in uniformly adsorbed N3/ZrO2/CL photoanodes. The result of 18 hours N3/ZrO2/ZnO CL DSSC shows the best fill factor of 0.56 with Voc of 487 mV, Jsc of 0.72 mA/cm2 and efficiency of 0.2 %. The influence of dye loading time of 18 hours significantly improves the Voc of the cell by 36.8 % with respect to 6 hours of dye loading time. Also, the prepared solar cell with CL shows enhanced solar cell parameter values than without it.

Influence of Dye Loading Time on Zirconia Photoanode for Solar Cell Application