The paper presents the results of the influence of the variation in the ratio of zinc and titanium oxide components in the mechanochemical production of perovskite-like ceramics based on zinc titanate, as well as the influence of the variation of the sintering temperature on the processes of phase formation and changes in the optical and electrochemical parameters of ceramics. It has been shown that a change in the stoichiometric ratio of the initial components has a significant effect on the kinetics of mechanochemical processes, as well as on the formation of the phase composition, including the formation of a perovskite-like ZnTiO3 phase. It has been established that deviation from stoichiometry leads to a change in the defect structure of the material, including the formation of oxygen vacancies and distortions of the crystal lattice, which, in turn, affects its functional characteristics. During the studies conducted, the influence of variation in the annealing temperature on the kinetics of phase transformations associated with the formation of a stable ZnTiO3 phase and transformations of the TiO2 – anatase → TiO2 – rutile type was determined. It has been established that the formation of the ZnTiO3 phase and its subsequent structural ordering occurs at a sintering temperature of 600 °C and above, while at a temperature of 900 – 1000 °C, coarsening of ceramic grains occurs due to recrystallization processes that occur during phase formation. It has been established that the formation of the ZnTiO3 phase leads to an increase in the value of Pmax to 0.3 – 0.4 W×cm2, which is achieved at a current density of about 0.35 - 0.5 A×cm-2, which are optimal operating conditions in which polarization losses are minimal.