Influence of Local Non‑Potable Water Sources on Cement Paste Properties Under Two Curing Regimes

Burachat Chatveera1

Hafiz Waheed Iqbal2

Mohammad Alameri3

Qudeer Hussain4

Panuwat Joyklad5,6, Email

Satish Paudel7

Panumas Saingam8

Gritsada Sua-Iam9

1Department of Civil Engineering, Faculty of Engineering, Thammasat University (Rangsit campus), Pathum Thani, 12121, Thailand
2Department of Civil Engineering, COMSATS University Islamabad, Wah, Punjab, 47030, Pakistan
3Civil Engineering Department, College of Engineering and Architecture, Umm Al-Qura University, Makkah, 21955, Saudi Arabia
4Civil Engineering Department, Kasem Bundit University, Bangkok, 10510, Thailand
5Department of Civil and Environmental Engineering, Faculty of Engineering, Srinakharinwirot University, Nakhonnayok, Nakhon Nayok, 26120, Thailand
6Center of Excellence in Rail System Technology and Civil Engineering Material Innovation for Sustainable Infrastructure, Strategic Wisdom and Research Institute, Srinakharinwirot University, Bangkok, 10110, Thailand
7Department of Civil Engineering, Institute of Engineering, Tribhuvan University, Kathmandu, Bagmati, 44700, Nepal
8Department of Civil Engineering, School of Engineering, King Mongkut's Institute of Technology Ladkrabang, Bangkok, 10520, Thailand
9Department of Civil Engineering, Faculty of Engineering, Rajamangala University of Technology Phra Nakhon, Bangkok, 10800, Thailand 

 

Abstract

The research paper investigates the influence of different types of locally available water such as potable, sanitary, river, sea and canal water on the nature of cement paste under two curing conditions. The canteen water from Thammasat University, river water of Chao Phraya, seawater in Chonburi Province, and Khlong Nueng (Canal 1) canal water in Pathum Thani Province, Thailand, were used as a source of sanitary water. To determine the mechanical performance and behavior related to durability, flexural strength, compressive strength and water absorption tests on cement paste were performed on both standard 28 days water curing and on combined 28 days water curing and 2h heat curing at 200 °C. The potable water mix (CPW100) showed a water absorption of 9.82% under standard curing in water for 28 days. On the other hand, the water absorption of sanitary water mixes (CSNW) was higher, with 11.61% water absorption for CSNW25 mixture. Absorption was generally lower in mixes made with sea water (CSW) under standard curing conditions, such as 6.80% in CSW25 and 7.05% in CSW50.The compressive strength with normal curing was approximately 24-30 MPa under canal and sanitary water mixes and 38-50 MPa under river and sea water mixes, and strength development was clearly dependent on water chemistry. The control mix with potable water (CPW100) exhibited a flexural strength of 3.97 MPa at standard curing conditions. The sanitary water mixes at lower replacement level, that is CSNW25 and CSNW50 have higher flexural strength of 6.20 MPa and 6.25 MPa, respectively. 

Influence of Local Non‑Potable Water Sources on Cement Paste Properties Under Two Curing Regimes