Interfacial Energy Dissipation and Damping Enhancement in Adhesively Bonded Nitinol–Aluminium Hybrid Laminates: An Experimental and Numerical Study

Bakytzhan Sariyev1,2, Email

Alina Abdykadyr3

Yeldar Otynshiev3

Boris Golman3

Andas Amrin4,5

ChungKet Thein6 

Christos Spitas7

1School of Engineering and Applied Sciences, Harvard University, Cambridge, Massachusetts, 02138, United States of America
2Department of Science and Innovation, Astana IT University, Astana, 010000, Kazakhstan
3School of Engineering, Nazarbayev University, Astana, 010000, Kazakhstan
4Nazarbayev University Research Administration, Nazarbayev University, Astana, 010000, Kazakhstan
5Institute of New Materials, Almaty, 041605, Kazakhstan
6Department of Mechanical, Materials and Manufacturing Engineering, University of Nottingham Ningbo, Ningbo, Zhejiang, 315000, China
7Department of Aerospace Engineering, University of Nottingham, University Park, Nottingham, NG7 2RD, United Kingdom

 

Abstract

Adhesive bonding offers a low-temperature route for integrating Nickel–Titanium (NiTi) with Aluminium (Al) without high-temperature interfacial reactions, but the role of laminate architecture in damping remains insufficiently quantified. Here, two NiTi–Al laminates were fabricated from 0.25 mm sheets using a flexible nitrile-rubber contact adhesive: a NiTi–Al bilayer (NA) and a NiTi–Al–NiTi sandwich (NAN). Free-vibration cantilever tests with laser displacement sensing yielded first-mode damping ratios and natural frequencies by logarithmic decrement; monolithic Al and NiTi beams of nominally matched metal-stack thickness were tested as references. NA showed 12% and 16% above 0.50 mm Al and NiTi, respectively. NAN showed 72% above NA, with its first natural frequency between the 0.75 mm monolithic references. COMSOL eigenfrequency predictions agreed with experiment within about 8%. An analytical Ross-Kerwin-Ungar (RKU) model treating the adhesive as a viscoelastic shear layer was calibrated against the excess damping above the monolithic baseline. The model identifies adhesive shear as one contributor to dissipation but does not reproduce the measured excess-damping ratio between the two architectures, which indicates additional mechanisms. The results establish adhesive bonding as a viable route to lightweight NiTi–Al laminate structures with raised damping and identify the symmetric sandwich architecture as the main lever.

Interfacial Energy Dissipation and Damping Enhancement in Adhesively Bonded Nitinol–Aluminium Hybrid Laminates: An Experimental and Numerical Study