This study investigated the long-term performance of slag-based fiber-reinforced cementitious composites containing ground granulated blast furnace slag (GGBS) and cellulose fiber (CF) under CO2 and air curing. Samples were divided into three groups: Ordinary portland cement (OPC), GGBS, and GGBS-CF. Results showed that GGBS and GGBS-CF experienced mass loss under both curing conditions, whereas OPC lost mass in air but gained mass under CO2 curing. In terms of shrinkage, GGBS-CF exhibited the lowest shrinkage in air curing, while OPC showed the lowest shrinkage under CO2 curing. For carbonation resistance, OPC had a shallower carbonation depth than both GGBS and GGBS-CF, indicating slower CO2 penetration. At 91 days under air-curing conditions, GGBS-CF and GGBS achieved compressive strengths 31.0% and 28.5% higher than OPC, respectively. A similar trend was observed in flexural strength, with GGBS-CF showing a 33.9% increase, while GGBS remained comparable to OPC. Under CO2 curing, OPC exhibited improved mechanical properties, whereas both slag-based mixtures showed reduced strength, suggesting greater alteration of slag-derived hydrates than portlandite-rich systems. TGA revealed a pronounced carbonate decomposition peak at 700-800 °C, and XRD confirmed increased carbonate formation after CO2 exposure. These findings provide guidance for optimizing CO2 curing in sustainable cementitious materials.